(1) partial welding: it may be caused by incorrect welding position or problems in welding gun searching. At this time, it is necessary to consider whether the TCP (torch center point position) is correct and adjust it. If this happens frequently, it is necessary to check the zero position of each axis of the robot and correct the center zero.
(2) undercut: it may be caused by improper selection of welding parameters, incorrect welding gun angle or position, which can be adjusted properly.
(3) air hole problem: it may be caused by poor gas protection, too thick primer of workpiece or wrong position, which can be adjusted properly.
(4) too much spatter: it may be caused by improper selection of welding parameters, gas component reasons or too long external audit length of welding wire. The power of the robot can be adjusted properly to change the welding parameters, the gas proportioner can be adjusted to adjust the proportion of mixed gas, and the relative position of welding gun and workpiece can be adjusted.
(5) a crater is formed at the end of the weld after cooling: when programmable, the submerged arc can be added to the working step to fill it up.